Carbon Fibers length ?

Status
Not open for further replies.

Fred

Materials
Sep 2, 1999
45
Is there any specification on Carbon Fibers length in material like PA66 15% CF
 
Replies continue below

Recommended for you

Not as far as I know, except for internal QC at individual compounders.

High aspect ratio and high surface area are important qualities in being good reinforcements though.

All carbon fibre I have seen has had a very fine fibre, which helps obtain both the above

Regards
pat
 