Is there any specification on Carbon Fibers length in material like PA66 15% CF
 
Not as far as I know, except for internal QC at individual compounders.

High aspect ratio and high surface area are important qualities in being good reinforcements though.

All carbon fibre I have seen has had a very fine fibre, which helps obtain both the above

Regards