Good day,

I am on the retrofitting project, and I resorting in to two methods

1. to use a carbon fiber to reinforced the prestressed slab
2. to use a steel plate with epoxy resins

Its the first time that I encounter these method. Do you have any good references or sample design regarding these methods?

thank you in advance

Poems are made by fools like me, but only God can make a tree. engineers creates wonderful buildings, but only God can creates wonderful minds
 
Replies continue below

Recommended for you

The best resource texts I have used for carbon fibre strengthening include:

ACI440.2 "Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Concrete Structures".

A textbook by Lawrence Bank "Composites for Construction Structural Design with FRP Materials".

Concrete Society Technical Report 55 "Design Guidance for Strengthening Concrete Structures Using Fibre Composite Materials".

Is there anything in particular you are looking into?
 
Agree with Kikflip - I've used all three in the past and found them very helpful.

Regards,
Qshake
[pipe]
Eng-Tips Forums:Real Solutions for Real Problems Really Quick.
 
i found some references on carbon fibers and so on,but mostly they are guide on designing beam having carbon fiber inside the concrete,not outside the beam

i am also looking for a sho-bond method,but i cant find useful resources regarding these method

Poems are made by fools like me, but only God can make a tree. engineers creates wonderful buildings, but only God can creates wonderful minds
 
Jenofstructures - All of the references above are for placing a FRP product on concrete beams externally and are not for fiber-reinforced concrete. If you are strengthening a concrete beam, slab, or column, I suggest using those references.

I am not familiar with the sho-bond method.

Regards,
Qshake
[pipe]
Eng-Tips Forums:Real Solutions for Real Problems Really Quick.
 
thanks