Hi,
What is the minimum allowable value of carbon equivalent for ASTM A105 fittings?

thanks in advance.
 
There is no minimum (or maximum) carbon equivalent in the ASTM A 105 specification. There are maximum values for some elements but the specification is based around achieving the required mechanical properties.
 