Jan 20, 2006 #1 nuke1973 Mechanical Joined Jan 2, 2006 Messages 7 Location TR Hi, What is the minimum allowable value of carbon equivalent for ASTM A105 fittings? thanks in advance.
Hi, What is the minimum allowable value of carbon equivalent for ASTM A105 fittings? thanks in advance.
Jan 20, 2006 #2 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US There is no minimum (or maximum) carbon equivalent in the ASTM A 105 specification. There are maximum values for some elements but the specification is based around achieving the required mechanical properties. Upvote 0 Downvote
There is no minimum (or maximum) carbon equivalent in the ASTM A 105 specification. There are maximum values for some elements but the specification is based around achieving the required mechanical properties.
Jan 20, 2006 #3 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US see thread292-145140 Upvote 0 Downvote