We have an Acetic Acid Above Surface Storage Tank made of 6.5 mm thick plates of A240-316L. We recently observed corrosion and pitting up to 1 mm deep on tank plates at what appears to be grinding marks used to remove weld spatter at the time of commissioning. Apparently manufacturer used grinder suitable for CS plates on tank plates hence resulting in carbon contamination.
We are planning to prevent further corrosion on these corrosion sites by either passivation or appropriate paint system application. Based on your experience please share which is the more suitable option of the two and is there any other option available to us to prevent further corrosion.
Regards
We are planning to prevent further corrosion on these corrosion sites by either passivation or appropriate paint system application. Based on your experience please share which is the more suitable option of the two and is there any other option available to us to prevent further corrosion.
Regards