Hi ,We have tried some solution annealing of 316 forged bolts to meet the requirements as per ASTM A193 B8M CL.1. Observed hardness before solution treatment was 38HRC .Parts has heated to 1050Deg for 1 hour and water cooled.Hardness has dropped to 125HBW after treatment. We will perform a tension test and corrosion test on these now.Now the concern is hardness has dropped and achieving a minimum tensile of 515MPa as per ASTM A193 B8M with this hardness seems to be very difficult.We expect to get a hardness above 150HBW . Is there anything we can do on the current solution treatment process to achieve this hardness- like changing time /temperature or an aging will work on this ?