We are considering the fabrication of a pressure vessel being lined through the explosion bonding process.
This vessel needs to be PWHT.
Our concern is carbide precipitation into the liner from the PWHT.
Specs:
Vessel shell and heads ,,, SA516
Vessel thickness,,,,,,,,,, 45-57 mm
Liner,,,,,,,,,,,,,, Alloy 59 (N06059)
Liner thickness,,,,,,,,,,,,,3 mm
Liner to nozzles,,,,,,,,,, Alloy 59 TIG welding overlay.
PWHT procedure temp,,,,,,, 570 C
Process,,,,,,,,,,,,,,,,,,,Versatic Acid
Operating conditions: 95 bar, 200 C.
Is Carbide Precipitation into the liner and it's surface a concern?
Thanks in advance.
This vessel needs to be PWHT.
Our concern is carbide precipitation into the liner from the PWHT.
Specs:
Vessel shell and heads ,,, SA516
Vessel thickness,,,,,,,,,, 45-57 mm
Liner,,,,,,,,,,,,,, Alloy 59 (N06059)
Liner thickness,,,,,,,,,,,,,3 mm
Liner to nozzles,,,,,,,,,, Alloy 59 TIG welding overlay.
PWHT procedure temp,,,,,,, 570 C
Process,,,,,,,,,,,,,,,,,,,Versatic Acid
Operating conditions: 95 bar, 200 C.
Is Carbide Precipitation into the liner and it's surface a concern?
Thanks in advance.