When attaching thermocouples to pressure boundary via capacitance discharge welding the energy output should be limited to 125 W-S as per ASME Sec 8 Div. 2. Why is this limitation? To what extent can it be lowered below 125 w-s?
 
Please do not cross post with other forums.
thread794-437611
 