I have a small and expensive weldment that I would like to convert into a cast or PM part. I have seen this done and welded to mild steel but don't know what material or process was used to make the part. Part will be welded to a 1" mild steel shaft.
Looking for suggestions.
Thanks
David
Looking for suggestions.
Thanks
David