Can you suggest me alternate low cost Track pin material
I am facing availability issue with SAE 4140
 
In my experience 4140 is the lowest alloy product that works for these pins.
Are you buying tube or bar?
There are a number of US sources, but low cost is not part of that supply chain.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy
 