Thanks guys. But I've a question for moldcore. Tell me how does Al. load up the filters more than other metals? I presume 10 or 20 micron filters are used in EDM machines. So for the filters to get loaded up, Al has to produce larger size residues. If this is true, is there any method of reducing the particle size?