I'm trying to figure out what BS (British standard) L65 Aluminum converts to. Possibly 2024 T??? Thanks for the help!!
 
Replies continue below

Recommended for you

Take a look at this thread. The CASTI Red Book would be a good place for authoritative conversions of BS aluminium grades to ASTM, SAE, etc.

thread2-178465
 
L65 was replaced by 2L77 and L168
2L77 is 2014A Forging stock and forgings
L168 is 2014A Bars and sections