Guys I need some way to attach some type of a 304L/316L stainless forged pipe fitting, e.g. a weldolet or coupling, to a cast part. The part in question is the volute of a centrifugal pump.
Can I weld directly to the cast volute? I would like to use a SMAW stick procedure, position weld in the field, but I can TIG them on if I have to. What about some other method of attachment, e.g. brazing or silver solder? (Don't suggest J-B weld ;-) )
Thanks for your help and ideas! Pete
Thanks!
Pete
Can I weld directly to the cast volute? I would like to use a SMAW stick procedure, position weld in the field, but I can TIG them on if I have to. What about some other method of attachment, e.g. brazing or silver solder? (Don't suggest J-B weld ;-) )
Thanks for your help and ideas! Pete
Thanks!
Pete