Can anhydrous ammonia ?vapor or liquid?cause erosion or corrosion for piping elbow and tee made of carbon steel or low alloy steel in refrigeration system?
 
sounds like contamination in the system.
Is there much water? Check the pH?

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
In high velocity flow pattern (<erosion velocity), the anhydrous ammonia may not have a specific synergetic effect to accelerate the corrosion while amine or ammonium bisulfide has an accelerative effect of corrosion.

The most critical issue will be Stress Corrosion Cracking, not a severe metal loss if the design is under the general erosion velocity limitation.

References
- NACE Publication 24061
- MTI MS-6
 