Hi fellow members. I am specifying a camlock Type-A adaptor threaded to a CS pipe nipple for firewater application. The adaptor is there for the vac truck to connect to whenever line draining is required. The camlock Type-A adaptor is only available in brass, aluminum or SS material. My question is, which of these is a better material to recommend to the vendor knowing that there will be different materials connected together? Appreciate input from your experiences on this. Thanks for the help.
 
Replies continue below

Recommended for you

I would go for brass myself to avoid any issue with galvanic corrosion and because it looks nice when polished.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Hi LittleInch - thank you very much for your quick feedback. You are surely a very active and knowledgeable member of this group and I follow your responses on other posts very keenly. Thanks again.
 