Looking into possibilities to replace cadmium plating in aerospace environment, fasteners bolts nuts etc. (Material stainless steel in contact with aluminum parts.
Specially for suppliers who can offer service of plating.

Does anybody has experience with AlMg Platings on steel
 
Replies continue below

Recommended for you

smanseif

Try
IVD aluminum AMS2427
Zn-Ni Plating AMS2417
Regards, Wil Taylor
 