I consistently run into dimensioning problems on parts required to have Cad Plating per QQ-P-416 on close tolerance
diameters.(.0005 inch or less)My question is: How can you allow a tolerance for plating without effectivly eliminating most of the tolerance for machining? For Example, Class 3 plating is .0002 minimum per side or .0004
on the diameter. If you allow only .0003 maximum plating per side you wind up with a variation of .0004 to .0006 on the diameter for the plating itself. with .0003 tolerance for machining.