Hello all!

I have a question regarding the "Explanatory Notes" in the A23.3-14 Concrete Handbook. I'm designing a plain concrete square footing and section N22.6.6 shows the following calculation for Shear resistance:

Vr = 0.18*λ*Φc√f'c*(lb/Q)

What does the "Q" in the above equation reference here? I do not see any info on this in the handbook. I'm also assuming the "l" and "b" is the length and width of the footing? Thank you.
 
Replies continue below

Recommended for you


I do not think so ..although i do not have a copy of the CAC Concrete Design Handbook. Assuming the plain concrete section shall be un-cracked section, the subject formula should be derived from famous max . shear stress ( pls look any strength og materials , solid mechanics ..etc ) v= VQ/(I*b).

My opinion is , Q at the Vr = 0.18*λ*Φc√f'c*(lb/Q) is Q is the statical moment of the area, I = moment of inertia , and b is thickness ( in this case width of the ftg)


Just saying ..