Does anyone have any good references for the rough equivalent for US steel grades against those from Europe? In particular I'm looking at C60.
 
Replies continue below

Recommended for you

Hi Boiler8019,
I believe Machinery Handbook has a fairly extensive list. For this type of enquiry it is best to get on the phone to a local Steel Supplier. They have the specifications on their PCs. That way you get the answer the same day (with a website it could take weeks for someone to respond).

Regards - Sgt Johnp