Does anyone have any good references for the rough equivalent for US steel grades against those from Europe? In particular I'm looking at C60.
 
Hi Boiler8019,
I believe Machinery Handbook has a fairly extensive list. For this type of enquiry it is best to get on the phone to a local Steel Supplier. They have the specifications on their PCs. That way you get the answer the same day (with a website it could take weeks for someone to respond).

Regards - Sgt Johnp