We have experienced this problem for several years and with different motors.The problem is usually limited to burnt motor leads at the Star connection.These motors are 5 Kv induction motors.The Star point 3 leads in some cases are bolted together and taped,on other motors ,the 3 leads are brought to a large copper busbar in the Motor JBox and bolted individually.These too burn near the STAR point from time to time.
This problem have not caused any motor breakdowns (yet)and the problem is usually found when motor is removed for OHaul or other.Do any of you have an idea or a similar problem.
Thanks a lot.
GusD