rconnor
Mechanical
- Sep 4, 2009
- 556
We've got issues with our oil baffles in a bearing for a hydroelectric units shaft. The baffle is made of Buna-N and after about a year the baffle swells, becomes wavy and, in some cases, shears off at its mounting location. Also, the rubber that has been in-service can be torn by hand. The image attached shows a baffle that was removed from service after a 8000 hr (~1 year) inspection.
The baffle is attached at one end (you can see the drill holes in the image) and protrudes into the bearing to deflect the oil back into the oil pot. The oil is Teresso 32 turbine oil and the temperature would be around 50-75[C]. The forces on the baffle shouldn't be of any great impact.
Before I saw the baffle, I thought it might be ozone cracking because it's buna-n and is located near the generator. However, it doesn't appear to be the case after seeing it. They also thought that they just over-tightened the clamp but on the next unit they loosened it and the same thing happened.
I have very limited experience with rubbers and I'm not sure what is happening and why. According to some research I've done, Buna-N should be resistant to oil swelling but it is definitely obsorbing oil (the thickness increased significantly).
Any thoughts on what might be causing this and would a material change (to viton or something else) be needed?
Thanks in advance for any advice!
The baffle is attached at one end (you can see the drill holes in the image) and protrudes into the bearing to deflect the oil back into the oil pot. The oil is Teresso 32 turbine oil and the temperature would be around 50-75[C]. The forces on the baffle shouldn't be of any great impact.
Before I saw the baffle, I thought it might be ozone cracking because it's buna-n and is located near the generator. However, it doesn't appear to be the case after seeing it. They also thought that they just over-tightened the clamp but on the next unit they loosened it and the same thing happened.
I have very limited experience with rubbers and I'm not sure what is happening and why. According to some research I've done, Buna-N should be resistant to oil swelling but it is definitely obsorbing oil (the thickness increased significantly).
Any thoughts on what might be causing this and would a material change (to viton or something else) be needed?
Thanks in advance for any advice!