BS 4871 Part1 was superseded by BS EN 287-1: 1992.
There is/was no requirement for mechanical testing of welders test pieces, only for weld procedure qualification, which is covered by EN ISO 15614-1:2004.
This details test pieces , locations of test samples and the conditions under which impact tests are required. You need to get hold of copies of these standards.