Hi all,
I apologize if this is the wrong subforum for this. We are brazing a 441SS bushing (4mm thick) to a 441SS pipe (1mm thick). Our company has not done brazing before and I'm having trouble finding the appropriate filler material and flux to put on the drawing. The only requirements we would have is that it needs to be able to withstand at least 650°C and support vibrations you'd expect to see in a vehicle's exhaust system.
Any suggestion on what to go with? Thanks!
I apologize if this is the wrong subforum for this. We are brazing a 441SS bushing (4mm thick) to a 441SS pipe (1mm thick). Our company has not done brazing before and I'm having trouble finding the appropriate filler material and flux to put on the drawing. The only requirements we would have is that it needs to be able to withstand at least 650°C and support vibrations you'd expect to see in a vehicle's exhaust system.