Folks,
I have a question regarding fully brazed Aluminium plate finned heat exchangers, such as cold boxes (ethylene production plants), that have been in service for many years.
Is there any need (indeed and any way) to inservice inspect a fully brazed APFHE if they are fully insulated/fireproofed, have non degrading fluid services on all sides (e.g. ethylene, propylene, ethane), are not exposed to any mercury, have no indication of leaks, experience an average of one cyclic load per year, have piping arranged in such a way that referred forces are minimal but that have been in service for up to 40years???
API RP-572 and API510 and even our own inservice inspection code, AS3788 is fairly silent on the issue.
I'm struggling to come up with any justification to drive any kind of inspection, but that doesn't "feel" right.
Any thoughts?
I have a question regarding fully brazed Aluminium plate finned heat exchangers, such as cold boxes (ethylene production plants), that have been in service for many years.
Is there any need (indeed and any way) to inservice inspect a fully brazed APFHE if they are fully insulated/fireproofed, have non degrading fluid services on all sides (e.g. ethylene, propylene, ethane), are not exposed to any mercury, have no indication of leaks, experience an average of one cyclic load per year, have piping arranged in such a way that referred forces are minimal but that have been in service for up to 40years???
API RP-572 and API510 and even our own inservice inspection code, AS3788 is fairly silent on the issue.
I'm struggling to come up with any justification to drive any kind of inspection, but that doesn't "feel" right.
Any thoughts?