Dear All,

I am confused what QW-404.12 says regarding change in classification. Is it mandatory to use same brand if PQR is qualified with impact testing? If not can you explain why?



Regards,

Umair
 
No, trade name or brand has nothing to do with flux-electrode classification.
 