Hi Everyone,
My question is in regard to B31.3 FIG. 328.5.4D Acceptable Details For Branch Attachment Welds.
We have a fabricator that used sketch 1 where we had specified sketch 2. Will this adversely affect our design? I can't find anything in the code to suggest this. It seems both are acceptable as long as full penetration welds were done (and done correctly).
Background info if it matters:
Water Glycol Service
200 Deg F
150 PSI
36" C.S. Header 0.5" Thick
12" C.S. Branch 0.375 Thick
Modeled as Unreinforced Tee
SIFi=7.541, SIFo=9.721
My question is in regard to B31.3 FIG. 328.5.4D Acceptable Details For Branch Attachment Welds.
We have a fabricator that used sketch 1 where we had specified sketch 2. Will this adversely affect our design? I can't find anything in the code to suggest this. It seems both are acceptable as long as full penetration welds were done (and done correctly).
Background info if it matters:
Water Glycol Service
200 Deg F
150 PSI
36" C.S. Header 0.5" Thick
12" C.S. Branch 0.375 Thick
Modeled as Unreinforced Tee
SIFi=7.541, SIFo=9.721