Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Boss fitting or Thredolet 1

Status
Not open for further replies.

EGAtomic

Materials
Apr 24, 2014
11
I was wondering if any one could tell me what the advantages and disadvantages are between a boss fitting or thredolet, I am redesigning a 1" return line that requires a 1/4" threaded connection for an instrument and I saw that I could either use a threaded boss fitting or thredolet. I just want to know if there is an advantage to one or the other, thanks.
 
Replies continue below

Recommended for you

One disadvantage of olets that pops in my mind immediately is that they require a lot of weld metal, and may therefore warp your pipe due to high het input. Unless one takes a lot of cooling between each pass, or has a reasonably small pipe, olets cam be a time consuming weld and therefore expensive.
With a one inch run you might not run into problems though, using an olet.

Why not use 1x1/2 red tee, and a B16.11 1/4" half coupling?
 