Nov 1, 2010 #1 DOHC Automotive Joined Oct 17, 2010 Messages 8 Location NL Hi, I'm looking for a glue or bonding agent to bond stainless steel together strongly and able to withstand heat (1200F - 1500F) Any suggestions?
Hi, I'm looking for a glue or bonding agent to bond stainless steel together strongly and able to withstand heat (1200F - 1500F) Any suggestions?
Nov 1, 2010 Thread starter #3 DOHC Automotive Joined Oct 17, 2010 Messages 8 Location NL a little bit more info which product from 3m? oh and i forgot to add it's got to last a long time outdoor. Upvote 0 Downvote
a little bit more info which product from 3m? oh and i forgot to add it's got to last a long time outdoor.
Nov 1, 2010 #4 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,868 Location US CONTACT AN APPLICATIONS ENGINEER WITH A DETAILED DESCRIPTION OF YOU APPLICATION. Regards, Mike Upvote 0 Downvote
Nov 1, 2010 #5 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US I would contact the Graphite Store with your exact requirements. The alternate to adhesives is brazing. The type brazing will depend on the aesthetics required. The carry a very good cross section of high temperature adhesives. http://www.graphitestore.com/items_list.asp/action/prod/prd_id/1/cat_id/4 http://www.graphitestore.com/items_list.asp/action/prod/prd_id/3/cat_id/4 Upvote 0 Downvote
I would contact the Graphite Store with your exact requirements. The alternate to adhesives is brazing. The type brazing will depend on the aesthetics required. The carry a very good cross section of high temperature adhesives. http://www.graphitestore.com/items_list.asp/action/prod/prd_id/1/cat_id/4 http://www.graphitestore.com/items_list.asp/action/prod/prd_id/3/cat_id/4
Nov 1, 2010 Thread starter #6 DOHC Automotive Joined Oct 17, 2010 Messages 8 Location NL Thanks i'll contact them. Upvote 0 Downvote
Nov 1, 2010 #7 btrueblood Mechanical Joined May 26, 2004 Messages 10,035 Location US "The alternate to adhesives is brazing" ...or welding. Upvote 0 Downvote
Nov 3, 2010 #8 USAeng Mechanical Joined Jun 6, 2010 Messages 419 Location US This may be something similar to what you are looking for? http://aremco.com/a3.html Upvote 0 Downvote