ahmadramadan
Structural
- Jul 18, 2015
- 8
I would like to calculate the bond between concrete and steel sections(steel tubes,etc)
I found one paper which define the bond relationship (Experimental Study on Shear Splitting Failure of Full-Scale
Composite Concrete Encased Steel Beams)
and I found fs=51.25629.544p
where p =steel area to section area
fs= bond stress between concrete and steel
So my questions are
1.I found in AISC 16.1-95 that reduction safety factor of 0.45 for bond between concrete and steel, but this is for filled composite member not encased(encased mean the tubes are not filled inside with concrete),so is there any section dealing with encased in the AISC (Hence I need this factor to use in the previous paper equation)
2.My second question the equation bond strength by AISC (In the same page is not clear to me ,variables are not clear, can anyone simplify it
Thank you
I found one paper which define the bond relationship (Experimental Study on Shear Splitting Failure of Full-Scale
Composite Concrete Encased Steel Beams)
and I found fs=51.25629.544p
where p =steel area to section area
fs= bond stress between concrete and steel
So my questions are
1.I found in AISC 16.1-95 that reduction safety factor of 0.45 for bond between concrete and steel, but this is for filled composite member not encased(encased mean the tubes are not filled inside with concrete),so is there any section dealing with encased in the AISC (Hence I need this factor to use in the previous paper equation)
2.My second question the equation bond strength by AISC (In the same page is not clear to me ,variables are not clear, can anyone simplify it
Thank you