Jun 10, 2020 #1 jreep1973 Structural Joined Oct 28, 2013 Messages 13 Location US What types of bolts should be used when bolting aluminum clips to a structural steel member?
Jun 10, 2020 #2 kingnero Mechanical Joined Aug 15, 2009 Messages 1,783 Location BE In a corrosive environment? Upvote 0 Downvote
Jun 10, 2020 Thread starter #3 jreep1973 Structural Joined Oct 28, 2013 Messages 13 Location US Kingnero: It will be an exterior stair connecting to a steel frame. So only exposed to the outdoor elements but NOT near the coast. Upvote 0 Downvote
Kingnero: It will be an exterior stair connecting to a steel frame. So only exposed to the outdoor elements but NOT near the coast.
Jun 10, 2020 #4 kingnero Mechanical Joined Aug 15, 2009 Messages 1,783 Location BE Is the structural steel hot dip galvanised or otherwise coated? Upvote 0 Downvote
Jun 10, 2020 Thread starter #5 jreep1973 Structural Joined Oct 28, 2013 Messages 13 Location US Kingnero: The structural steel is painted. Not galv. Upvote 0 Downvote
Jun 10, 2020 #6 kingnero Mechanical Joined Aug 15, 2009 Messages 1,783 Location BE Do you have any more information that might be of interest to us? Like the clips are anodised perhaps? Upvote 0 Downvote
Do you have any more information that might be of interest to us? Like the clips are anodised perhaps?
Jun 10, 2020 Thread starter #7 jreep1973 Structural Joined Oct 28, 2013 Messages 13 Location US The aluminum is mill finished and not anodised. I'm not sure of the aluminum make up, but the structural steel is A992 Gr. 50ksi and I believe the steel is painted. Upvote 0 Downvote
The aluminum is mill finished and not anodised. I'm not sure of the aluminum make up, but the structural steel is A992 Gr. 50ksi and I believe the steel is painted.
Jun 10, 2020 #8 r13 Civil/Environmental Joined Oct 26, 2019 Messages 5,988 Location US The aluminum is mill finished and not anodised. Click to expand... The aluminum may corrode, consider to coat it. Upvote 0 Downvote
The aluminum is mill finished and not anodised. Click to expand... The aluminum may corrode, consider to coat it.
Jun 11, 2020 #9 Tmoose Mechanical Joined Apr 12, 2003 Messages 5,636 Location US Is this a commercially purchased stair from a well established manufacturer?? Are the "clips" provided by the stair manufacturer ? Upvote 0 Downvote
Is this a commercially purchased stair from a well established manufacturer?? Are the "clips" provided by the stair manufacturer ?
Jun 12, 2020 #10 mfgenggear Aerospace Joined Jan 23, 2008 Messages 3,611 Location US what is the purpose of the clips Upvote 0 Downvote