JamyFilter
Mechanical
Hello,
Does anyone know if bolts class 12.9 can be used at a temperature of 350 [°C] with design code AD-2000?
As per first information, an inspector told us upper limit is 300 [°C].
Thanks a lot for your reply. If you can supply, I am interested in the reference you use to reply.
Regards
Does anyone know if bolts class 12.9 can be used at a temperature of 350 [°C] with design code AD-2000?
As per first information, an inspector told us upper limit is 300 [°C].
Thanks a lot for your reply. If you can supply, I am interested in the reference you use to reply.
Regards