Should I expect any "problems"? Thanks.
 
Replies continue below

Recommended for you

Galvanic corrosion is the usual concern with dissimilar metal joints. As far as vibration resistance, that is usually a function of the threaded fastener geometry and preload level generated.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
If there is motion between the two parts, you may get wear on the aluminum part preferentially, loosening up the joint and leading to failure.
 