Jun 28, 2016 #1 azzt Mechanical Joined May 19, 2004 Messages 32 Location GB Hi I have a precision steel bolt M10 x 1.25 and it has a raised letter q on the head. I'm fairly sure this is Japanese. Can anyone tell me if this relates to the material strength or is it something else? Thanks in advance allan
Hi I have a precision steel bolt M10 x 1.25 and it has a raised letter q on the head. I'm fairly sure this is Japanese. Can anyone tell me if this relates to the material strength or is it something else? Thanks in advance allan
Jun 28, 2016 #2 SwinnyGG Mechanical Joined Jan 22, 2016 Messages 2,600 Location US Just a raised letter Q, or are their other markings? (dots, lines, any other shapes or letters) Upvote 0 Downvote
Jun 28, 2016 #3 EdStainless Materials Joined May 20, 2004 Messages 16,373 Location Waukesha WI USA There used to be a database of bolt IDs. Though I have been searching and haven't found it. I hope someone with a better memory than mine comes along. I had thought that it was part of a DoD report on bogus fasteners... = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote
There used to be a database of bolt IDs. Though I have been searching and haven't found it. I hope someone with a better memory than mine comes along. I had thought that it was part of a DoD report on bogus fasteners... = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube
Jun 28, 2016 #4 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,867 Location US Ed, I got this from the fora previously, MIL-HDBK-57E. Don't think the OP's maker is listed, but can't say for sure. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand http://files.engineering.com/getfile.aspx?folder=928b6563-bedd-4f70-83a4-d09f77a3567a&file=MIL-HDBK-57E.pdf Upvote 0 Downvote
Ed, I got this from the fora previously, MIL-HDBK-57E. Don't think the OP's maker is listed, but can't say for sure. Regards, Mike The problem with sloppy work is that the supply FAR EXCEEDS the demand
Jun 28, 2016 #5 SnTMan Mechanical Joined Jan 22, 2005 Messages 6,867 Location US Here's another, same source The problem with sloppy work is that the supply FAR EXCEEDS the demand http://files.engineering.com/getfile.aspx?folder=7a21769c-c497-4dc5-acf0-f74c944be284&file=fasteneridentificationguide.pdf Upvote 0 Downvote