May 16, 2014 #1 bhart192 Civil/Environmental Joined Feb 6, 2006 Messages 81 Location US what asme code covers UT inspection of boiler tube welds
May 16, 2014 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Boiler tube butt welds are exempt from volumetric examination (UT) based on Section I, Table PW-11. All the information is there. Upvote 0 Downvote
Boiler tube butt welds are exempt from volumetric examination (UT) based on Section I, Table PW-11. All the information is there.
May 19, 2014 #3 weldstan Materials Joined Jun 24, 2011 Messages 2,808 Location US Assuming that the Owner is specifying volumetric examination, acceptance criteria must be agreed upon between Manufacturer/Contractor and Owner. Upvote 0 Downvote