what asme code covers UT inspection of boiler tube welds
 
Replies continue below

Recommended for you

Boiler tube butt welds are exempt from volumetric examination (UT) based on Section I, Table PW-11. All the information is there.
 
Assuming that the Owner is specifying volumetric examination, acceptance criteria must be agreed upon between Manufacturer/Contractor and Owner.
 