Blow Molding Foot Pump

Status
Not open for further replies.

ThinkSnow247

Mechanical
Jun 2, 2004
6
I am working on designing a small baffled foot pump. It is designed to be blow molded out of a soft rubber or plastic. We were planning on molding the pump out of santoprene. However we want to be able to store the pump with all the baffles compressed. We learned that the baffles will not spring back after they are stored compressed for an extended period of time if made from santoprene. What are are some similar materials that will remain elastic over time and can be blow molded?
 
Replies continue below

Recommended for you

I think Santoprene has the lowest creep and best elastic recovery of any thermoplastic elastomer. If Santoprene won't cut it, then you will need a thermoset elastomer. As far as I know, thermosets cannot be blow moulded

Regards
pat pprimmer@acay.com.au
eng-tips, by professional engineers for professional engineers
Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor