Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Blending of EVA with 2 different Vinyl Acetate content

Status
Not open for further replies.

Zed Megan

Chemical
Oct 21, 2020
1
Hi guys, Good morning!

Can somebody kindly assist me in understanding about my concern.
Is it possible to blend 2 EVA with different vinyl acetate content?
What are the effects if we blend these two in EVA photovoltic film sheet for Solar panel.

Like for example VA 28% and VA 20%

Thanks in advance guys!
 
Replies continue below

Recommended for you

The final properties of the mixture will follow the rule of mixtures. This means that, for example, the Tg of the mixture will be intermediate between the Tg of the individual components.
 