I'm looking for a resource that can apply the black overlay to four trim pieces. The material is rigid about 6-mils thick.

Arrow(s) below:

1) Just showing the location of the trim as reference
2) Top is trim as it should be... Bottom is the black overlay removed.



Questions?

Help?

XJ_Reveal_SW_lmtnhv.jpg
 
You could talk to powder coaters, but the masking will be tricky.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Are you sure the parts are stainless steel? Typically those parts are plastic moldings with electroplated copper + nickel + chromium.

The black color usually is an adhesive tape, such as those provided by Avery Denison or 3M:




A typical high-volume applicator would be Tesa:

 
409 stainless is very common for these trim pieces, but your tape comments still apply Cory.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 