I'm searching for the properties of this obsolete shape, specifically web and flange thicknesses, any help would be appreciated.

Thanks
 
Replies continue below

Recommended for you

From AISC Steel Design Guide 15:

B15x38.5
A = 11.26 sq in
d = 15.00 in
tw = 0.29 in
bf = 6.75 in
tf = 0.535 in
T = 12.868 in
k = 1.066 in
X1 = 2222 ksi
Ix = 442.4 in^4
Sx = 59.0 in^3
rx = 6.27 in
Iy = 24.1 in^4
Sy = 7.2 in^3
ry = 1.46 in
Zx = 66.2 in^3
Zy = 11.5 in^3
J = 0.95 in^4
Cw = 1261 in^6

This is a 1922-1930 beam fabricated by Bethlehem
 
Here is a reference supplied by strc in thread367-87056
"Thanks for the link, I couldn't find info I was looking for but I found it in a really good reference book: "Structural Renovation of Buildings" by Alexander Newman which I warmly recommend for reconstruction projects".
 