What is the best valve material for a high performance drone engine, have tried 17-4ph does not do well at higher temps (above 900F) valve diameter is .54 for intake .49 for exhaust. The engines I have developed are a four valve per cylinder Dual Overhead Cam boxter twin similar to a BMW motorcycle. We are curently developing a larger version of 270 cc. I have tried to find SAE EV8 (UNS 63008) have not had any luck, it seems to only be availabe to valve mfg. that have this alloyed...... any ideas??? would "Nitronic 60" that has been Ion Nitrided be a good choice????
We manufacture these engines from the ground up that includes almost all parts of the engine minus screws and bearings
Thanks
Cofactors
We manufacture these engines from the ground up that includes almost all parts of the engine minus screws and bearings
Thanks
Cofactors