We are putting Ag/Zn batteries into a metal can and need resistance to KOH(1.3-1.45 sg)to prevent leakage, strength to resist deformation against internal pressure, and potentially electrical isolation. Any ideas on testing or references to the best previous work published?
Thanks, Tom