MechAnalyst2112
Aerospace
I need a high strength u-bolt of 3/4" rod dia and 4-1/2" inner diameter. I planned on using A325 rod with rolled threads, and then bend to correct inner diameter. The part will also be galvanized.
However, another engineer metioned that this would result in hydrogen embrittlement due to the stress after bending in the high strength steel.
If this is true, can anyone suggest a method/process to get a high-strength steel u-bolt without getting the hydrogen embrittlement issue????
However, another engineer metioned that this would result in hydrogen embrittlement due to the stress after bending in the high strength steel.
If this is true, can anyone suggest a method/process to get a high-strength steel u-bolt without getting the hydrogen embrittlement issue????