Hello,

I'm looking for a formula that describes the bending behavior of Aluminum (in function of Al-type thickness, shape,…); I want to know at what bending angle aluminum starts to deform (so not springs back to his initial position).

Thanks
R. Litz
 
test...

Unless You are dealing with "annealed or low-alloyed" aluminum there WILL be a critical minimum bend-radius and a minimum "spring-back" factor in every case. Note: for virtually every alloy/temper combination [or "similar-to" combination] this data is published. I use company data so I can't send you numbers; however, many aircraft sheet metal fab manuals have this data.

Note: simple bend-tests should confirm min BR and spring-back for various samples.

NOTE: this data is usually valid for STRAIGHT-LINE bends using constrained tooling, such as a "break" with radiused edges. Caution: bends thru a curve CAN present different challenges!!!

NOTE: deburr edges carefully and examine outer BR surfaces and edges with 10X--50X magnification for signs of cracking [NDI if questionable]. Regards, Wil Taylor
 
When the material Yield strenght is excceed, then permanent deformation takes place
 
I had the same question in the past and someone gave me a bending calculator software is pretty handy and it helps to reduce testing. email me and I'll send it to you