tc7
Mechanical
- Mar 17, 2003
- 387
We will need to bend 1” thick 4340 normalized bar stock through a 5/8” inside radius. Later in the process, we will be welding on this component and perform a post weld Q&T to increase final strength to ~165-170 uts.
I am worried about the initial 5/8” radius bend and by the way the bar is bent through a full 180 degrees. Is it recommended this be heated as part of the bending operation? If so what might be a recommended temperature?
Is there any reason to think this needs to be bent in two steps with a stress relief (or normalization?) between each step; for instance bend through 90 degrees then SR (or normalize?), then bend through to the full 180 degrees and SR again (or normalize?)
>>>> Regarding the post weld Q&T operations, can anyone advise what the martensite finish temperature is for 4340? I will need to know this as p/o my upcoming weld procedure qualification.
Advice and experience welcomed.
Thankyou
I am worried about the initial 5/8” radius bend and by the way the bar is bent through a full 180 degrees. Is it recommended this be heated as part of the bending operation? If so what might be a recommended temperature?
Is there any reason to think this needs to be bent in two steps with a stress relief (or normalization?) between each step; for instance bend through 90 degrees then SR (or normalize?), then bend through to the full 180 degrees and SR again (or normalize?)
>>>> Regarding the post weld Q&T operations, can anyone advise what the martensite finish temperature is for 4340? I will need to know this as p/o my upcoming weld procedure qualification.
Advice and experience welcomed.