The inside bend radius is a function of the tool used to make it. In general, you should use an inside bend radius at least 1.5 * material thickness. However, what you specify may not be what is available. Check the radii of the available tools and select from those. You might want a .045" radius but you'll likely not find it. The tools we used had nose radii of .030, .060, .090, etc.
- - -Dennyd, P.E.