Oct 2, 2013 #1 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US Does anyone know of a reference I could go to to get bearing strength as a function of temperature for 6061-T651 and 2219 T852 aluminum?
Does anyone know of a reference I could go to to get bearing strength as a function of temperature for 6061-T651 and 2219 T852 aluminum?
Oct 8, 2013 Thread starter #2 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US how about any correction factor charts? Upvote 0 Downvote
Oct 9, 2013 #3 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US I doubt that this data exists in the public domain. I think you can get yield and tensile vs. temperature from MIL-HDBK-5 or MMPDS-0X. Use the ratio of bearing:tensile at room temp and apply this ratio to the high temp value. Upvote 0 Downvote
I doubt that this data exists in the public domain. I think you can get yield and tensile vs. temperature from MIL-HDBK-5 or MMPDS-0X. Use the ratio of bearing:tensile at room temp and apply this ratio to the high temp value.
Oct 10, 2013 Thread starter #4 kevlar49 Materials Joined Jun 1, 2006 Messages 287 Location US thanks tvp. aren't the temperature correction factors in MMPDS only for modulus in the case of 6061 and tensile properties for 2219? Upvote 0 Downvote
thanks tvp. aren't the temperature correction factors in MMPDS only for modulus in the case of 6061 and tensile properties for 2219?