Does anyone know of a reference I could go to to get bearing strength as a function of temperature for 6061-T651 and 2219 T852 aluminum?
 
how about any correction factor charts?
 
I doubt that this data exists in the public domain. I think you can get yield and tensile vs. temperature from MIL-HDBK-5 or MMPDS-0X. Use the ratio of bearing:tensile at room temp and apply this ratio to the high temp value.
 
thanks tvp. aren't the temperature correction factors in MMPDS only for modulus in the case of 6061 and tensile properties for 2219?
 