The common tin-base and lead-base babbits are specified in ASTM B23. For high performance rotating equipment,tin-base is the choice, and the lead should be specified as low as possible.
For ASTM B23, Babbit types /melting temperature deg F
1 433
3 464
4 363
5 358
7 464
10 468
11 471
12 473
16 471
19 462